Availability: | |
---|---|
Application:
Drilling mud and oil based pipe free agent in oil fields.
Usage:
Feed the 881-A dry powder and distribute it according to sludge recipe.
Dosage:
881-A’s dosage in the system is usually 2-5% (percentage in weight)
Common chemical, physical properties
Composition | Montmorillonite organic ammonium derivative |
Appearance | Light white fine powder |
Moisture content (%) | ≤3.5 |
Dry powder fineness (through mesh 200) | ≥99 |
Loss on ignition (900C,%) | 32~34 |
Colloid fraction % | >95 |
Package & Storage:
Kraft paper bag interior with PE .
The weight : 25±0.25kg per bag.
The package and weight also can be customized.
Product should be stored in ventilated, cool and dry place.
Storage life : two years.
Application:
Drilling mud and oil based pipe free agent in oil fields.
Usage:
Feed the 881-A dry powder and distribute it according to sludge recipe.
Dosage:
881-A’s dosage in the system is usually 2-5% (percentage in weight)
Common chemical, physical properties
Composition | Montmorillonite organic ammonium derivative |
Appearance | Light white fine powder |
Moisture content (%) | ≤3.5 |
Dry powder fineness (through mesh 200) | ≥99 |
Loss on ignition (900C,%) | 32~34 |
Colloid fraction % | >95 |
Package & Storage:
Kraft paper bag interior with PE .
The weight : 25±0.25kg per bag.
The package and weight also can be customized.
Product should be stored in ventilated, cool and dry place.
Storage life : two years.